Process for preparing alumina being suitable for layer chromatography

US4225639A · kind A · utility

8Cited by
6References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 19, 1979
Grant dateSep 30, 1980
Priority date
Expiry dateJun 19, 1999

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG01N30/93
  • WIPO fieldMeasurement
  • WIPO sectorInstruments

Abstract

The invention relates to a process for preparing alumina being suitable for layer chromatography. The alumina suitable for layer chromatography is prepared in accordance with the invention in such a manner that an aluminium trinydroxyde containing 34 to 37% by weight of bayerite, 3 to 5% by weight of pseudoboehmite and 60 to 62% by weight of amorphous aluminium trihydroxide is heated at 300.degree. C. to 400.degree. C. for 2 to 4 hours. The activated alumina thus produced is snow-white, has a large specific surface and its average grain size is within the range between 8 and 20 .mu.m. The product complies with the requirements of layer chromatographical technique.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.