Amorphous alloy with high magnetic induction at room temperature
US4226619A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | May 4, 1979 |
| Grant date | Oct 7, 1980 |
| Priority date | — |
| Expiry date | May 4, 1999 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01F1/153
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
An amorphous alloy including iron, carbon and boron characterized by exceptional magnetic induction properties at room temperature, rendering it particularly suitable for use as the core of a power transformer. The alloy includes 83 to 90 atomic % iron, 2 to 13 atomic % carbon, and 4 to 15 atomic % boron, the total boron and carbon content ranging from 10 to 17 atomic %. If desired, up to 10% of the iron can be replaced by cobalt or nickel, while up to 2% of the carbon can be replaced by silicon or germanium.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.