Patent · US Expired

Heat-treated zirconium alloy product

US4226647A · kind A · utility

7Cited by
3References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 12, 1978
Grant dateOct 7, 1980
Priority date
Expiry dateJun 12, 1998

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/30
  • WIPO fieldEngines, pumps, turbines
  • WIPO sectorMechanical engineering

Abstract

High tensile strength, creep and corrosion resistant zirconium alloys containing 7.0-10.0 wt % aluminum, 0-3 wt % in total of one or more elements selected from the group consisting of magnesium, tin, chromium, iron, carbon, silicon, yttrium, niobium, molybdenum and beryllium, the balance zirconium and incidental impurities, are produced by annealing cast alloys at a temperature below about 992.degree. C. for a period of time sufficient to produce alloys having a substantially continuous matrix of the ordered intermetallic compound Zr.sub.3 Al. The alloys may initially be hot worked at temperatures about 1000.degree. C., while in the .beta.Zr-Zr.sub.2 Al two phase region, prior to annealing. Preferred alloys contain 7.5-9.5 wt % aluminum, the balance zirconium and incidental impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.