Method of operation of a refractory fiber production process
US4238213A · kind A · utility
50Cited by
12References
5Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 5, 1979 |
| Grant date | Dec 9, 1980 |
| Priority date | — |
| Expiry date | Apr 5, 1999 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03B37/055
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An improved process for the centrifugal spinning of refractory fibers is described. In the improved process rotor circumferential speeds of at least about 21,000 linear feet per minute (6,400 linear meters per minute) are used. In a preferred embodiment the circumferential surfaces of the rotors are also inclined from being perpendicular to the axis of the molten stream, preferably by about 8.degree. to 20.degree..