Porous nickel coated electrodes
US4251344A · kind A · utility
Assignee
Inventor
Key dates
| Filing date | Jan 22, 1980 |
| Grant date | Feb 17, 1981 |
| Priority date | — |
| Expiry date | Jan 22, 2000 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/50
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
An improved electrode having a surface mixture of nickel and porous nickel produced by applying a paste mixture of NiAl.sub.2 and Ni.sub.3 B together with a vehicle to a substrate. After burning off the vehicle and firing in air at a temperature of 450.degree. to 650.degree. C. and thereafter sintering at a temperature of 800.degree. to 900.degree. C. in nitrogen, the coating on the substrate contains Ni.sub.2 Al.sub.3, NiAl.sub.2 B and nickel together with a thin overlayer of B.sub.2 O.sub.3. After removing the intermetallic aluminum, boron and boron oxide by dissolution with sodium hydroxide, the surface of the substrate contains Raney nickel supported on a structure of nickel. The resulting electrodes can be used as cathodes in water or brine electrolysis cells.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.