Low shrinkage polyester resin compositions
US4251641A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Dec 4, 1979 |
| Grant date | Feb 17, 1981 |
| Priority date | — |
| Expiry date | Dec 4, 1999 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L67/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Unsaturated polyester resin compositions that have a low shrinking property, and at the same time, an enough strength are provided. The compositions comprises (1) 30-70 parts by weight of an unsaturated polyester obtained by reactin terephthalic acid and/or isophthalic acid and one or more of unsaturated acids selected from the group consisting of maleic anhydride, maleic acid and fumaric acid, with a glycol, and having the unsaturation degree of 1.5-5.0 and the acid value of 18-40, (2) 70-30 parts by weight of .alpha.,.beta.-ethylenically unsaturated monomer, and (3) 5-30 parts by weight of an amorphous linear saturated polyester resin obtained by reacting terephthalic acid and/or isophthalic acid with a glycol component.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.