Abstract
A method of preparing a mixture of cation and anion exchange resins in the size range of about 10 to 250 microns, comprising combining cation exchange resins and anion exchange resins of a size larger than 60 mesh and grinding the combination of anion and cation exchange resins to a size range of about 10 to 250 microns.