Abstract
The improvement of passing an inert, preferably vaporizable and condensible, liquid material through or over a polyester molten mass in a polymer reactor to further increase surface area-to-volume ratio and/or lower the partial pressure of vaporous products of condensation so that viscosity of the polymer is increased at a substantially greater rate in the same residence time is taught for the prior art condensation process in a film-forming reactor at temperatures of 275.degree. C. to 300.degree. C., pressures of 0.1 to 760 Torr, and residence times of 0.1 to 6 hours. A polymer having an intrinsic viscosity above 0.65, preferably over 0.7, is produced.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.