Patent · US Expired

Method for overaging of hot dip metal coated steel material

US4294632A · kind A · utility

4Cited by
1References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 24, 1979
Grant dateOct 13, 1981
Priority date
Expiry dateSep 24, 1999

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D9/52
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Method for overaging hot dip metal coated steel material to improve formability, comprising rapidly heating the material to a temperature of above 300.degree. C. but below that at which the coating is undesirably denatured at heating rate of at least 50.degree. C./sec., followed by controlled slow cooling of cooling rate of not more than 20.degree. C./sec. Total processing time required can be one or two minutes, thus the method can be continuously carried out.