Method of manufacturing rolled steel products with high elastic limit

US4295902A · kind A · utility

9Cited by
3References
4Claims
0Family size

Assignee

Inventor

Key dates

Filing dateFeb 26, 1980
Grant dateOct 20, 1981
Priority date
Expiry dateFeb 26, 2000

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D1/02
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A rolled steel product is given an elastic limit of 500 to 1200 MPa by selection of a particular steel composition and a particular heat treatment. The steel contains 0.10-0.50% C, 0.90-1.50% Mn, and 0.10-0.45% Si, and optionally 0.20-0.70% Ni, 0.10-0.80% Cr, and 0.02-0.10% V. The heat treatment consists of surface quenching from above the austenitization temperature by means of a fluid, the heat remaining in the product being sufficient to temper the martensite and/or bainite in the quenched surface.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.