Air-drying, fatty acid-modified lacquer binders, based on fumaric or maleic acid bis-glycidyl ester copolymers
US4304695A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Aug 25, 1980 |
| Grant date | Dec 8, 1981 |
| Priority date | — |
| Expiry date | Aug 25, 2000 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F2810/30
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A binder composition which has a number average molecular weight of from 1000 to 20,000 and which comprises, in copolymerized form, from 5 to 55% by weight of fumaric acid and/or maleic acid bis-glycidyl ester and from 95 to 45% by weight of one or more vinyl and/or vinylidene monomers, esterified to an acid number of from 3 to 30 mg KOH/g with from 18 to 72% by weight, based on copolymer plus fatty acid, of a fatty acid and subsequently reacted with 0 to 3% by weight, based on copolymer plus fatty acid plus dicarboxylic acid anhydride, of a dicarboxylic acid anhydride.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.