Aromatic thermoplastic polyphosphonatocarbonate
US4322520A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 18, 1980 |
| Grant date | Mar 30, 1982 |
| Priority date | — |
| Expiry date | Jun 18, 2000 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G64/083
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Thermoplastic polyphosphonatocarbonate prepared by polycondensing at least one aromatic dihydroxy compound with a diaryl carbonate and a phosphonic acid diaryl ester in the presence of a basic polycondensation catalyst at a temperature of from 80.degree. to 340.degree. and under a pressure of 600 to 0.1 mm Hg in an inert gaseous atmosphere, the molar ratio of diaryl carbonate to phosphonic diaryl ester being from 5:95 to 95:5 and the molar ratio of aromatic dihydroxy compound to the sum of diaryl carbonate and phosphonic acid diaryl ester being from 0.91:1 to 0.99:1, and following polycondensation, neutralizing said basic catalyst.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.