Additive for air-entrained super plasticized concrete, concrete produced thereby and method of producing air-entrained super plasticized concrete

US4328145A · kind A · utility

17Cited by
1References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 26, 1979
Grant dateMay 4, 1982
Priority date
Expiry dateOct 26, 1999

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B24/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Air entrained, super plasticized concrete having a maximum bubble spacing factor of 0.008 inch (ASTM Standard C 457) and a method for preparing such concrete are disclosed. The method includes the steps of adding an air entraining agent while mixing aggregates and water, adding during the mixing a small but effective quantity of a potassium salt of a fluorinated alkyl carboxylate having a high surface activity and a pH of 8-9, and then adding a super plasticizer to the resulting mix prior to placement. The air entrained concrete having the aforesaid bubble spacing factor contains a super plasticizer, a vinsol resin air entraining agent, and a potassium salt of a fluorinated alkyl carboxylate. The fluorinated alkyl carboxylate is present in an amount of one to two parts per 100 parts of the super plasticizer on a weight basis.