Method of synthesizing zincosilicate or stannosilicate or titanosilicate material

US4329328A · kind A · utility

34Cited by
3References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 16, 1980
Grant dateMay 11, 1982
Priority date
Expiry dateOct 16, 2000

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01B39/08
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Sodium zinco/stanno/titano-silicate is synthesized by mixing a concentrated aqueous sodium zincate, stannate or titanate solution with a source of silica (e.g. powdered glass or sodium metasilicate solution) in the ratio 60 g sodium silicate to sodium zincate equivalent to 8.1 g zinc oxide, keeping the temperature at 40.degree. C. for 1/2 hour, diluting threefold with water of 20.degree. C., allowing a precipitate to form overnight, and filtering and drying the residue at 110.degree. C. The resulting sodium zincosilicate may be used in its own right as a water softener or may be converted by cation exchange into any other desired zincosilicate.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.