Superficially hydrolyzed biocompatible polyamide material
US4336357A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 28, 1980 |
| Grant date | Jun 22, 1982 |
| Priority date | — |
| Expiry date | Jul 28, 2000 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S128/03
- WIPO fieldMedical technology
- WIPO sectorInstruments
Abstract
Polyamide materials for the construction of protheses and surgical sundries are made biocompatible by inducing a superficial hydrolysis by treating such materials, either raw or in the form of shaped articles, with a normal multiple solution of hydrogen chloride. Thrice normal or fourfold normal solutions are preferred and the treatment time being a function of the temperature. At human body temperature (37.degree. C.) a treatment time from 30 to 60 minutes will do.