Patent · US Expired

Scheelite flotation

US4366050A · kind A · utility

2Cited by
10References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 19, 1981
Grant dateDec 28, 1982
Priority date
Expiry dateJan 19, 2001

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB03D2203/04
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A scheelite concentrate is recovered from a scheelite ore containing silicate minerals and other calcareous minerals by froth flotation which process comprises grinding the ore sufficiently fine to liberate the scheelite grains, pulping the gound ore with water to form a slurry containing between about 20% and about 40% solids by weight, sequentially conditioning the slurry with at least one alkali metal carbonate in small but effective amounts to provide an alkaline pH adjustment and a source of carbonate ions, with small but effective amount of alkali metal silicates to depress siliceous and calcareous gangue minerals other than scheelite and with a fatty acid collector in small but effective amounts to coat the scheelite grains, the conditioning with the fatty acid collector being conducted with sufficient agitation to disintegrate floccules of scheelite, silicate mineral and other calcareous mineral grains and to preferentially reflocculate the scheelite grains for a period of time sufficient to produce upon flotation a concentrate having a grade of at least about 50% WO.sub.3, adding a frother to the collector conditioned slurry and subjecting the collector conditioned slurry …

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.