Abstract
Premilled semichloro copper phthalocyanine or partially sulfonated semichloro copper phthalocyanine is slurried and stirred with sulfuric acid (50-60% and preferably 55-59% in the case of semichloro copper phthalocyanine and 50-61% and preferably 58-61% in the case of partially sulfonated semichloro copper phthalocyanine) at 50.degree.-85.degree. C., preferably 65.degree.-75.degree. C. for 1/2 to 4 hours. The slurry is diluted with to less than 35% sulfuric acid concentration and stirred at 60.degree.-95.degree. C. for 1/2 to 4 hours. The resulting highly transparent pigment is filtered and dried.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.