Method of producing elongated large-size forged article
US4404041A · kind A · utility
6Cited by
6References
22Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Oct 29, 1982 |
| Grant date | Sep 13, 1983 |
| Priority date | — |
| Expiry date | Oct 29, 2002 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T29/49988
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of producing forged article by casting a molten alloy steel containing 0.02 to 0.15 wt % of niobium and 9 to 12 wt % of chromium in a metal mold to form an ingot and subjecting the ingot to a forging. The ingot is formed to have a diameter greater than the height thereby to prevent generation of eutectic NbC and sedimental crystals.