Method of producing spherical lithium aluminate particles

US4405595A · kind A · utility

24Cited by
9References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 15, 1982
Grant dateSep 20, 1983
Priority date
Expiry dateJan 15, 2002

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Spherical particles of lithium aluminate are formed by initially producing aluminum hydroxide spheroids, and immersing the spheroids in a lithium ion-containing solution to infuse lithium ions into the spheroids. The lithium-infused spheroids are rinsed to remove excess lithium ion from the surface, and the rinsed spheroids are soaked for a period of time in a liquid medium to remove water and NH.sub.4 OH from their surfaces. The soaked spheroids are then dried and sintered to form lithium aluminate spherical particles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.