Preparing P.sub.2 S.sub.5 of low reactivity
US4419104A · kind A · utility
2Cited by
4References
2Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 2, 1981 |
| Grant date | Dec 6, 1983 |
| Priority date | — |
| Expiry date | Jul 2, 2001 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01B25/14
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Phosphorus pentasulfide of low reactivity is made by solidifying molten phosphorus pentasulfide on a cooling cylinder that delivers the solidified product at a temperature of 150.degree. to 220.degree. C., and that product is immediately introduced into a heat-insulated container and freed therein from its immanent or sensible heat by cooling at a rate of at most 30.degree. C. per hour without the expenditure of any energy to control the cooling.