Process for the preparation of cellular polyurethane elastomers based on 4,4'-diisocyanato-1,2-diphenylethane
US4421870A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 20, 1982 |
| Grant date | Dec 20, 1983 |
| Priority date | — |
| Expiry date | Sep 20, 2002 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G2410/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The invention relates to a method for the preparation of cellular polyurethane elastomers with densities of approximately 250 to 800 grams per liter by reacting 4,4'-diisocyanato-1,2-diphenylethane or a diisocyanato-1,2-diphenylethane isomer mixture with a 4,4'-diisocyanato-1,2-diphenylethane content of more than 95 percent by weight with higher molecular weight polyhydroxyl compounds and water, as well as optionally chain extenders in the presence of auxiliaries and/or additives according to the one-shot or preferably the prepolymer method in closed molds. Compared with products based on 4,4'-diisocyanatodiphenylmethane, the polyurethane elastomer molded parts have improved physical and thermal properties.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.