Process for hard coating with sorbitol and products obtained thereby
US4423086A · kind A · utility
48Cited by
5References
22Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 16, 1981 |
| Grant date | Dec 27, 1983 |
| Priority date | — |
| Expiry date | Jun 16, 2001 |
Classification
- Technology area (CPC A)Human Necessities
- CPC primaryA61K9/2826
- WIPO fieldPharmaceuticals
- WIPO sectorChemistry
Abstract
Process for hard coating with sorbitol. On the one hand, a sorbitol syrup having a concentration of 60 to 85% by weight is supplied on a moving bed of cores to be coated and, on the other hand, the temperature prevailing in the bed is kept at a value comprised between 50.degree. and 10.degree. C. The present coating process applies conveniently to cores of the "without sugar" type in the field of confectionery and pharmaceutical products.