Filtrate reducer additive for swelling clay grouts and cement-swelling clay grouts

US4424290A · kind A · utility

2Cited by
5References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 13, 1981
Grant dateJan 3, 1984
Priority date
Expiry dateAug 13, 2001

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09K17/48
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

An additive for swelling clay grouts and cement-swelling clay grouts, intended to reduce the filtrate, lower and stabilize viscosity, retard rigidification time, limit sweating and sedimentation of the solid constituents, is an alkaline ethylenic acid polymer and/or copolymer, with molecular weight between 500 and 20,000, but preferably between 1000 and 6000. This additive is especially advantageous in the fields of civil engineering, building, public works and drilling.