Method of recovering uranium oxide from alkaline sodium uranyl carbonate solutions
US4436704A · kind A · utility
5Cited by
4References
6Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 24, 1982 |
| Grant date | Mar 13, 1984 |
| Priority date | — |
| Expiry date | Jun 24, 2002 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01G43/025
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of recovering uranium dioxide from a sodium uranyl carbonate solution obtained by the alkaline carbonate leaching of uranium ore in which a solution is reacted at a temperature above 130.degree. C. and at superatmospheric pressure with particular metallic iron. The precipitated UO.sub.2 is recovered from the solution.