Diene/acrylate based impact modifier for PVC

US4443585A · kind A · utility

17Cited by
1References
10Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJul 12, 1983
Grant dateApr 17, 1984
Priority date
Expiry dateJul 12, 2003

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S525/902
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Impact modifiers having high efficiency at low levels and at low temperatures comprising at least three stages, Stage A being a non-crosslinked polymer of at least 70% butadiene and at least 10% lower alkyl (C.sub.2 -C.sub.8) acrylate, Stage B being a polymer of at least 80% styrene, and Stage C containing at least 50% methyl methacrylate and at least 1% alkyl (C.sub.1 -C.sub.4) acrylate, the ratio of Stages A:B:C, excluding optional additional stages, being about 70-85:10-15:10-20, the ratio of stages C:B being at least 1, and Stage A being non-agglomerated are disclosed. Also disclosed are methods of preparing the impact modifier and thermoplastic polymer compositions containing the impact modifier.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.