Patent · US Expired

Method of sizing hydrophobic yarn

US4448839A · kind A · utility

16Cited by
8References
13Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 20, 1981
Grant dateMay 15, 1984
Priority date
Expiry dateOct 20, 2001

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T442/2402
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

A method of sizing a hydrophobic yarn for weaving comprising the steps of applying thereto an acid pH latex of a free radical initiated vinyl polymer and drying the yarn. The polymer has a weight average molecular weight of from about 300,000 to about 2,500,000, and in dried film form is hydrophobic, not redispersible in a solution at a low pH and redispersible in an alkaline aqueous medium. The polymer is prepared from monomers comprising about 8% to about 14%, by weight ethylenically unsaturated acid. The average solubility parameter of the monomers in the polymer is between about 9.0 and about 9.5; the calculated polymer T.sub.g is between about -20.degree. C. and 20.degree. C. Preferred yarns are nylon and polyester.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.