Patent · US Expired

Hydrothermal pretreatment to prevent scale during liquefaction of certain solid carbonaceous materials

US4450066A · kind A · utility

7Cited by
8References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 8, 1982
Grant dateMay 22, 1984
Priority date
Expiry dateNov 8, 2002

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10G1/00
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

Scale formation during the liquefaction of lower ranking coals and similar carbonaceous materials is significantly reduced and/or prevented by hydrothermal pretreatment. The said pretreatment is believed to convert the scale-forming components to the corresponding carbonate prior to liquefaction. The said pretreatment is accomplished at a total pressure within the range from about 1000 to about 4400 psia. Temperature during said pretreatment will generally be within the range from about 500.degree. to about 700.degree. F.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.