Abstract

An early high-strength mineral polymer composition is formed of a polysialatesiloxo material obtained by adding a reactant mixture consisting of alumino-silicate oxide (Si.sub.2 O.sub.5,Al.sub.2 O.sub.2) with the aluminum cation in a four-fold coordination, strong alkalis such as sodium hydroxide and/or potassium hydroxide, water, and a sodium/potassium polysilicate solution; and from 15 to 26 parts, by weight, based upon the reactive mixture of the polysialatesiloxo polymer of ground blast furnace slag. Sufficient hardening for demolding is obtained in about 1 hour with this composition.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.