Method of minimizing slagging in the burning of black liquid
US4514256A · kind A · utility
Inventors
Key dates
| Filing date | Apr 18, 1983 |
| Grant date | Apr 30, 1985 |
| Priority date | — |
| Expiry date | Apr 18, 2003 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC10L10/06
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
The formation of slag is minimized and the removability of slag is greatly increased, in connection with the furnace burning of black liquor, by applying to the surfaces where slag tends to form a substance which, under black liquor furnace conditions, reacts with the sodium sulfide content of the black liquor ash to oxidize said sodium sulfide and to be itself reduced, such substances preferably comprising sodium persulfate, manganese dioxide, cupric oxide and ferric oxide and mixtures thereof.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.