Abstract
This invention relates to an anaerobic adhesive and method of making the same, comprising the reactive product of a glycidyl acrylate and a hydroxyl containing polyester. The reaction between the glycidyl acrylate and the polyester typically takes place in the presence of a radical inhibitor and an acid accelerator with oxygen present. The resulting adhesive is a single component, structural adhesive which will cure in an anaerobic environment.