Process for producing fibrous assembly
US4526735A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 9, 1983 |
| Grant date | Jul 2, 1985 |
| Priority date | — |
| Expiry date | Feb 9, 2003 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S264/46
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A process and apparatus for producing a fibrous assembly. At least one fiber-forming polymer is extruded through a spinneret having numerous small openings. The process uses a die equipped with a spinneret having numerous closely spaced small openings and an opening ratio (.alpha.) of at least 30%. At least one fiber-forming polymer in the form of a shaped mass having a specified compression resistance is continuously stuffed into said die. Said shaped mass has a shape such that it measures more in one direction than in another. There is passed through the spinneret an electric current sufficient to give said fiber-forming polymer Joule heat required for cutting said polymer by partitioning members defining the numerous small openings of the spinneret. The cut fiber-forming polymer is taken up as fine streams. The present invention provides ultrathick aromatic polyamide fibers having an average cross-sectional area of about 0.01 mm.sup.2 to about 5 mm.sup.2 and comprising at least one fiber-forming aromatic polyamide and an inorganic or metallic fine powder or a fibrous material.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.