Abstract
The invention relates to a stabilized composition for coating glass containers, and to its method of use. The method involves the steps of heating the surface of a glass container to at least 800.degree. F., and spraying the surface of the glass with a glass coating formulation comprising monoalkyltin trihalide and about 0.5 to 10 parts by weight per hundred parts monoalkyltin trihalide of a solubilizing material.