Abstract
Blends of (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/.alpha.-olefin copolymer are used to prepare peelable seals having nearly constant and predictable peel strength over an extended heat seal temperature range. Some of the seals so produced also show stress whitening.