Patent · US Expired

Recovery of nickel and cobalt by controlled sulfuric acid leaching

US4541868A · kind A · utility

26Cited by
25References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 22, 1983
Grant dateSep 17, 1985
Priority date
Expiry dateJul 22, 2003

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22B23/043
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

According to the present invention, improved dissolution of nickel and cobalt and thus improved recovery of those desired metal values is achieved by modifying the ore recovery processes wherein sulfuric acid leaching at elevated temperatures is used to dissolve the nickel and cobalt. In particular, according to the present invention, processes are provided wherein the sulfuric acid and ore are contacted at substantially ambient temperature prior to subsequent heating to attain the elevated temperatures of the sulfuric acid leach. Practice of the present invention has been found to result in improved metal value recovery.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.