Cationic surface coating of flat glass

US4544395A · kind A · utility

17Cited by
4References
23Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMar 3, 1981
Grant dateOct 1, 1985
Priority date
Expiry dateMar 3, 2001

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of treating flat glass to reduce its vulnerability to scratching, e.g. during storage and/or transit, wherein a transparent film of a cationic surface active agent is adsorbed on the glass by applying an aqueous solution of the surface active agent to the glass on the production line and drying the glass. The solution may be applied to the glass after is has been washed, near the end of the production line, using for example an anionic surface active agent as detergent. Alternatively, a solution containing both a cationic surface active agent and an nonionic surface active agent as detergent may be applied to the glass to wash it, followed by rinsing with water and drying.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.