Antifoulants for thermal cracking processes
US4545893A · kind A · utility
31Cited by
8References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 20, 1984 |
| Grant date | Oct 8, 1985 |
| Priority date | — |
| Expiry date | Jul 20, 2004 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S585/95
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
The formation of carbon on metals exposed to hydrocarbons in a thermal cracking process is reduced by contacting such metals with an antifoulant selected from the group consisting of a combination of tin and aluminum, a combination of aluminum and antimony and a combination of tin, antimony and aluminum.