Process for bonding lignocellulose-containing raw materials with a prepolymer based on a urethane-modified diphenylmethane diisocyanate mixture
US4546039A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Apr 27, 1983 |
| Grant date | Oct 8, 1985 |
| Priority date | — |
| Expiry date | Apr 27, 2003 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31989
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A process for bonding lignocellulose raw materials using an isocyanate group-containing urethane-modified diphenylmethane diisocyanate mixture having a viscosity of 120 to 1000 mPas at 25.degree. C. and an isocyanate content of 15 to 33.6 percent by weight which is obtained by reacting a diphenylmethane diisocyanate mixture containing 10 to 75 percent by weight of 2,4'-diphenylmethane diisocyanate with 0.05 to 0.5 hydroxyl equivalents of a polyol per equivalent isocyanate group.