Process for the production of coarse particle mordenite
US4564512A · kind A · utility
3Cited by
5References
1Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Oct 1, 1982 |
| Grant date | Jan 14, 1986 |
| Priority date | — |
| Expiry date | Oct 1, 2002 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S423/25
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
There is produced coarse particle mordenite by treating a reaction mixture consisting essentially of on a molar basis 2.5-10 Na.sub.2 O, Al.sub.2 O.sub.3, 15-30 SiO.sub.2, 400-4000 H.sub.2 O, 5-30 NaCl in an autoclave at a temperature of 140.degree. to 180.degree. C. until formation of crystals separating the crystalline product, washing with water and drying.