Method for reducing oxidic iron ores in a rotary kiln
US4581061A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 6, 1984 |
| Grant date | Apr 8, 1986 |
| Priority date | — |
| Expiry date | Sep 6, 2004 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
In a reduction process carried out in a rotary kiln in which oxygen-containing gases are introduced by way of nozzles and at least a part of the highly volatile solid reductants are introduced from the discharge end so as to be distributed over a substantial region of the kiln bed, and any remaining balance of the reductants is fed jointly with the ore and the additives at the feed end, the formation of fusion deposits is prevented by the introduction of at least 60% of the reductants via the discharge end, and that at least a 60% portion of the reductants includes no more than 20% of the total reductant particulates having less than a 3 mm particle size.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.