Production of fiber-reinforced materials
US4590104A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 14, 1985 |
| Grant date | May 20, 1986 |
| Priority date | — |
| Expiry date | Feb 14, 2005 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08J2381/02
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
Fiber-reinforced materials are produced by impregnating continuous filaments with a melt of a polyarylene sulfide ketone, preferably one having a reduced viscosity .eta..sub.red of from 0.1 to 0.5 [dl.g.sup.-1 ], shaping the resulting semi-finished product to give a finished article and heating the latter for not less than 15 minutes at above the crystallite melting point of the polyarylene sulfide ketone, the latter undergoing crosslinking and its glass transition temperature Tg increasing by not less than 5.degree. C.