Patent · US Expired

Production of ferroboron by the silicon reduction of boric acid

US4602950A · kind A · utility

2Cited by
6References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 12, 1985
Grant dateJul 29, 1986
Priority date
Expiry dateSep 12, 2005

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C33/003
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

This is a process for producing a ferroboron containing 0.5-20% silicon and up to 4.5% carbon. This process utilizes the silicon reduction of B.sub.2 O.sub.3 and avoids excessive losses due to volatilization of B.sub.2 O.sub.3. It also results in a ferroboron which is substantially free from aluminum impurity. The process uses a mixture, which includes an iron-containing constituent, a silicon containing constituent, and boric acid. Preferably a molten pool is prepared and controlled to a temperature of 1100-1550 (and preferably 1100.degree.-1450.degree. C.) prior to the addition of the boric acid. At least some of the silicon constituent can also be injected into the molten pool along with the boric acid.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.