Thermal upgrading of residual oil to light product and heavy residual fuel
US4604188A · kind A · utility
19Cited by
9References
24Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jan 16, 1985 |
| Grant date | Aug 5, 1986 |
| Priority date | — |
| Expiry date | Jan 16, 2005 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC10G9/00
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
A method of upgrading residual oil includes cracking the residual oil at a severity which is between visbreaking and coking to produce a light cracked product and a heavy bottom product. The heavy bottom product is mixed with diluents and additives which improves the flow characteristics to produce a pumpable fuel.