Patent · US Expired

Method of making paper having improved tearing strength

US4609432A · kind A · utility

12Cited by
9References
28Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJun 15, 1984
Grant dateSep 2, 1986
Priority date
Expiry dateJun 15, 2004

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD21H17/42
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

The tearing strength of paper is improved by providing a furnish in which the fiber content is predominantly refined fiber with a minor amount, preferably 2 to 10 wt. %, of added unrefined fiber having incorporated therein a heat activatable bonding agent, particularly starch. The bonding agent adheres to and coats the added fiber without chemically reacting with the fiber. A cationic material, particularly polyethyleneimine, is premixed with the raw starch to cause it to adhere to the added fiber. During heat drying of the formed paper the starch is gelatinized to effect enhanced bonding of the added fiber.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.