Patent · US Expired

Regeneration of noble metal-highly siliceous zeolite with sequential hydrogen halide and halogen or organic-halogen compound treatment

US4645751A · kind A · utility

28Cited by
7References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 23, 1985
Grant dateFeb 24, 1987
Priority date
Expiry dateDec 23, 2005

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB01J38/44
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A process is described for rejuvenation of a deactivated highly siliceous noble metal-containing zeolite catalyst which contains agglomerated noble metals. The process comprises initially reducing the deactivated catalyst in hydrogen, pretreating the thus reduced catalyst with an inert gas stream containing about 0.001 to 10 weight percent hydrogen chloride, redispersing the noble metal with an inert gas stream containing about 0.001 to 10 weight percent Cl in the form of Cl.sub.2 or Cl-containing organic material, and subsequently reducing the catalyst. The Cl-treatments may optionally occur in the presence of oxygen or sources of oxygen.