Aluminum-lithium alloys and method

US4648913A · kind A · utility

43Cited by
7References
43Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 29, 1984
Grant dateMar 10, 1987
Priority date
Expiry dateMar 29, 2004

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An aluminum base alloy wrought product suitable for aging and having the ability to develop improved strength in response to an aging treatment without impairing fracture toughness properties is disclosed. The product is comprised of 0.5 to 4.0 wt. % Li, 0 to 5.0 wt. % Mg, up to 5.0 wt. % Cu, 0 to 1.0 wt. % Zr, 0 to 2.0 wt. % Mn, 0 to 7.0 wt. % Zn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities. The product has imparted thereto, prior to an aging step, a working effect equivalent to stretching an amount greater than 3% in order that, after said aging, improved strength and fracture toughness combinations are obtained.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.