Production of inorganic fiber products
US4650825A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | May 6, 1985 |
| Grant date | Mar 17, 1987 |
| Priority date | — |
| Expiry date | May 6, 2005 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G8/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
An improved process for the production of glass and mineral fiber products bonded with a phenolic resin in which an aqueous phenol-formaldehyde resin is applied to the inorganic fiber as the bonding agent which is formed with calcium hydroxide as condensation catalyst and the mixture is thermally cured, the improvement comprising prior to processing the aqueous phenol-formaldehyde resin is adjusted to a pH of 7.5 to 11 by addition of a base and sulfate ions are added in an amount of 80 to 200% of the stoichiometric amount required for bonding the calcium ions whereby the calcium ions are converted into a water-soluble complex stable for at least three hours without any precipitation and the products produced thereby.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.