Process for refining molten steel
US4652308A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 1, 1985 |
| Grant date | Mar 24, 1987 |
| Priority date | — |
| Expiry date | Oct 1, 2005 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21C7/06
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The invention provides a process for obtaining low-nitrogen steel by tapping molten steel from a converter without deoxidizing and by then deoxidizing the molten steel in a ladle refining furnace from which slag has been removed, and a process for obtaining low phosphorus steel by tapping molten steel from a converter without deoxidation at a tapping temperature lower than conventional processes, and by performing deoxidation and composition adjustment of the molten steel in a ladle refining furnace from which slag has been removed.