Patent · US Expired

Reduction in the adhesion to glass of thermoplastic, plasticized polyvinylbutyral molding compositions

US4663235A · kind A · utility

5Cited by
1References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 10, 1985
Grant dateMay 5, 1987
Priority date
Expiry dateMay 10, 2005

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/3163
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Reduction in the adhesion to glass of thermoplastic, plasticized polyvinylbutyral molding compositions, in particular sheeting, by the addition of a metal salt and/or metal chelate of an enolizable .beta.-diketone, or mixtures of these compounds, as an non-stick agent, preferably in amounts of 0.003 to 0.3% by weight, relative to the plasticized polyvinylbutyral. It is preferable to employ the non-stick agent in the form of a solution in the plasticizer. The use of the sheeting having an adhesion to glass reduced in accordance with the invention as a laminating layer for the production of glass laminates.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.