Method for producing oxidic sintered nuclear fuel bodies
US4671904A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 14, 1985 |
| Grant date | Jun 9, 1987 |
| Priority date | — |
| Expiry date | Feb 14, 2005 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E30/30
- WIPO fieldEngines, pumps, turbines
- WIPO sectorMechanical engineering
Abstract
UO.sub.2 base powder exhibiting any specific surface and crystallite diameter properties is mixed with rare earth (SE) oxide-containing powder, the particles of which exhibit at least in one surface layer, a crystal lattice of the fluorite type, with the stoichiometric composition (SE.sub.0.5, U.sub.0.5) 0.sub.2.00 and/or form it in sintering; and is compacted to form compacts which are sintered in a gas atmosphere with reducing action at 1500.degree. C. to 1750.degree. C. to form high-density sintered bodies.