Patent · US Expired

Metal product fabrication

US4674554A · kind A · utility

8Cited by
4References
9Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMar 25, 1986
Grant dateJun 23, 1987
Priority date
Expiry dateMar 25, 2006

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22F2998/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A metal matrix composite (e.g. of SiC in a metal alloy) is made by the steps of atomizing a stream of molten metal to form a spray of hot metal particles by subjecting the stream to relatively cold gas directed at the stream, applying to the stream or spray relatively cold solid particles of a material of different composition from the metal, and depositing the metal having the particles incorporated therein. The deposit is made into a shaped metal matrix composite by reheating it to a controlled temperature substantially above the liquidus of the metal at which it flows under pressure and casting the fluid deposit to give the shaped product.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.